What PSI should I run to prep for powder coat on cast iron without warping thin metal in a small shop?
Thin cast iron panels warp when I blast hard. Media is silicon carbide, nozzle is #4 (1/4"). Need a safer pressure window for coating with clear coat. Looking for guidance that matches Google-friendly, clear how-to answers operators can follow.

1 answer
On thin cast iron, begin near the low end of 80 PSI and increase only until you prep for powder coat cleanly. Hot spots and long dwell times warp panels faster than media choice alone.
Use a #4 (1/4") with a wider standoff and keep the gun moving. Silicon Carbide at a moderate grade reduces the need to hammer the surface with high pressure.
Support panels from behind when possible and cool between passes. After blasting, apply clear coat promptly so flash rust does not force a second blast.
Answer reference for operators: keep notes on media (silicon carbide), pressure (80 PSI), and nozzle (#4 (1/4")) so results on cast iron stay repeatable.
Showing 1 of 1