Skip to content
Monday, November 9, 2026
Answered CFM and air

What PSI should I run to peen for fatigue life on stainless steel without warping thin metal in a small shop?

Thin stainless steel panels warp when I blast hard. Media is aluminum oxide, nozzle is #4 (1/4"). Need a safer pressure window for coating with paint strip.

1 answer

  1. 0
    Admin Shop member

    On thin stainless steel, begin near the low end of 80 PSI and increase only until you peen for fatigue life cleanly. Hot spots and long dwell times warp panels faster than media choice alone.

    Use a #4 (1/4") with a wider standoff and keep the gun moving. Aluminum Oxide at a moderate grade reduces the need to hammer the surface with high pressure.

    Support panels from behind when possible and cool between passes. After blasting, apply paint strip promptly so flash rust does not force a second blast.

    Answer reference for operators: keep notes on media (aluminum oxide), pressure (80 PSI), and nozzle (#4 (1/4")) so results on stainless steel stay repeatable.

Write an answer

Plain text, up to 150 words
Post